Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultramid® Advanced T1000HG6 un - PA6T/6I-GF30 - BASF

Material Data Center offers the following functions for Ultramid® Advanced T1000HG6 un:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Ultramid A datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
Heat stabilized, partially aromatic polyphthalamide for injection molding with strong mechanical properties especially at elevated temperatures and excellent chemical resistance for highly stressed parts. Ultramid® Advanced T1000 HG6 can be characterized as compound with high strength and stiffness, very low water absorption and outstanding dimensional stability. It features a high melting point (320°C) and excellent melt stability.

Markets & applications
Automotive: Fuel system, cooling system, powertrain, Auto E&E, sensors, pumps, fuel cell
Industry goods: Pumps, compressors
Consumer goods: Home appliances, consumer electronics
Processing/Physical Characteristics乾燥/調湿単位テスト基準
ISO データ
成形収縮率, 平行 0.4 / * % ISO 294-4, 2577
成形収縮率, 直角 0.9 / * % ISO 294-4, 2577
機械的特性乾燥/調湿単位テスト基準
ISO データ
引張弾性率 11800 / 12000 MPa ISO 527
破壊応力 210 / 205 MPa ISO 527
破壊ひずみ 2 / 2 % ISO 527
シャルピー衝撃強さ, +23°C 60 / 55 kJ/m² ISO 179/1eU
シャルピー衝撃強さ, -30°C 55 / 55 kJ/m² ISO 179/1eU
ノッチ付きシャルピー衝撃強さ, +23°C 8 / 7 kJ/m² ISO 179/1eA
ノッチ付きシャルピー衝撃強さ, -30°C 7.5 / 7 kJ/m² ISO 179/1eA
熱的特性乾燥/調湿単位テスト基準
ISO データ
溶融温度, 10°C/min 320 / * °C ISO 11357-1/-3
ガラス転移点, 10°C/min 130 / * °C ISO 11357-1/-2
荷重たわみ温度, 1.80 MPa 275 / * °C ISO 75-1/-2
厚さhでの燃焼性 HB / * class IEC 60695-11-10
試験片の厚さ 0.8 / * mm -
電気的特性.乾燥/調湿単位テスト基準
ISO データ
比誘電率, 100Hz 4.4 / 3.4 - IEC 62631-2-1
比誘電率, 1MHz 4.6 / 3.8 - IEC 62631-2-1
誘電正接, 100Hz 124 / 153 E-4 IEC 62631-2-1
誘電正接, 1MHz 109 / 24 E-4 IEC 62631-2-1
表面抵抗率 * / >1E15 Ohm IEC 62631-3-2
耐電圧 43 / - kV/mm IEC 60243-1
耐トラッキング性 - / 600 - IEC 60112
その他の特性.乾燥/調湿単位テスト基準
密度 1440 / - kg/m³ ISO 1183
材料特有の特性乾燥/調湿単位テスト基準
ISO データ
粘度数 120 / * cm³/g ISO 307, 1157, 1628
試験片の成形条件.単位テスト基準
ISO データ
射出成形, 樹脂温度 350 °C ISO 294
射出成形, 金型温度 150 °C ISO 294
特殊な特性
成形加工法.
射出成形.
納入形状.
ペレット.
特殊な特性.
熱安定化.
な特性
Melt Strength
耐薬品性
General Chemical Resistance
アプリケーション
自動車, 電気電子
領域別の利用可能性
その他の情報
村遜速揃
PREPROCESSING
Pre/Post-processing, max. allowed water content: .05 %
Pre/Post-processing, Pre-drying, Temperature: 120 °C
Pre/Post-processing, Pre-drying, Time: 8 h

PROCESSING
injection molding, Melt temperature, range: 345 - 355 °C
injection molding, Melt temperature, recommended: 345 °C
injection molding, Mold temperature, range: 140 - 170 °C
injection molding, Mold temperature, recommended: 150 °C
injection molding, Dwell time, thermoplastics: 5 min
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.